TIALN COATING

Model: TIALN COATING

MULTILAYER COATING 3 MICRONS THICK. THE PLASMA IS OBTAINED FROM THE FUSION OF A TITANIUM/ALUMINIUM CATHODE. AN EXCELLENT COATING THAT GUARANTEE HIGH THERMAL RESISTANCE. IT HAS AN OXIDATION TEMPERATURE OF 800°C RESULTING IN A SURFACE HARDNESS OF 3400 VICKERS. THE FRICTION COEFFICIENT IS 0,45 AND ALLOWS CIRCULAR SAWS TO BE USED WITH EXCELLENT RESULTS EVEN IN CONDITIONS OF LIMITED OR MINIMAL LUBRICATION AND MISTING. IT IS PARTICULARLY SUITED TO HIGH ALLOY STEELS OF UP TO 1100 N/mm2, CUTTING CAST IRON, STAINLESS STEEL AND ALL MATERIALS THAT DEVELOP CONSIDERABLE HEAT.